KONVERSI CANGKANG SAWIT MENJADI BIO-OIL DENGAN METODE PYROLYSIS MENGGUNAKAN KATALIS CoMo/MINERAL ALAM (LEMPUNG CENGAR)
dc.contributor.author | Wati, Fitri | |
dc.contributor.author | Bahri Syaiful | |
dc.contributor.author | Aman | |
dc.date.accessioned | 2013-01-17T02:35:00Z | |
dc.date.available | 2013-01-17T02:35:00Z | |
dc.date.issued | 2013-01-17 | |
dc.description.abstract | Fuel is a very important energy resource in life, but at the present, crisis of fuel occurred due to the lack of fossil fuel in Indonesia. One way to overcome this case is to develop alternative energy resources, like bio-oil. Bio-oil is produced by pyrolysis of biomass without the presence of oxygen. Biomass used in this research is shell of palm. The purpose of this research is to produce bio-oil as an alternative energy by pyrolysis shell of palm and to explain the effect of CoMo catalyst on yield of bio-oil. Catalyst concentration was varied from 0%, 0.5%, 1% to 1.5% w / w to biomass. Bio-oil formed was analyzed by GCMS and physics tests. 50 grams of biomass shell oil with a size of -60 +40 mesh, silinap 500 ml, and the catalyst CoMo / Clay 1.5 grams introduced into the slurry reactor, and pyrolysis process performed on the operating conditions of temperature 320 oC and stirring speed of 300 rpm with a flow of nitrogen gas (N2) as an inert gas. The results showed that the optimum yield obtained is 50,4 % at the concentration of catalyst CoMo 1.5%. The properties of bio oil produced has density 1.016 kg/m3, viscosity 22.83 cSt, acid value 68.34, flash point 85 oC. From analysis of chemical constituents by GC-MS, bio-oil produced constitutes 5.91% methanol, 2-propanone 2.73%, Acetic acid 54.91%, 17.63% Phenol, Furfural 6.64 %. The results obtained have characteristics approaching the characteristics of standard fuel oil and bio-oil. | en_US |
dc.description.sponsorship | en_US | |
dc.identifier.other | nurasmi | |
dc.identifier.uri | http://repository.unri.ac.id:80/handle/123456789/1484 | |
dc.language.iso | other | en_US |
dc.subject | Bio-Oil | en_US |
dc.subject | Shell Oil | en_US |
dc.subject | Catalyst Como / clay | en_US |
dc.subject | Pyrolysis | en_US |
dc.title | KONVERSI CANGKANG SAWIT MENJADI BIO-OIL DENGAN METODE PYROLYSIS MENGGUNAKAN KATALIS CoMo/MINERAL ALAM (LEMPUNG CENGAR) | en_US |
dc.type | student Paper Post Degree | en_US |
Files
Original bundle
1 - 1 of 1
No Thumbnail Available
- Name:
- Karya Ilmah_Fitri Wati (0807121198)_Teknik Kimia_2013_Konversi Cangkang Sawit.pdf
- Size:
- 979.6 KB
- Format:
- Adobe Portable Document Format
License bundle
1 - 1 of 1
No Thumbnail Available
- Name:
- license.txt
- Size:
- 1.71 KB
- Format:
- Item-specific license agreed upon to submission
- Description: