Efek Variasi Suhu Annealing Terhadap Morfologi Nanotube ZnO yang Di-doping Boron
dc.contributor.author | Pajrin, Erawati | |
dc.contributor.author | Iwantono | |
dc.contributor.author | Umar, Akrajas Ali | |
dc.date.accessioned | 2016-01-30T03:42:12Z | |
dc.date.available | 2016-01-30T03:42:12Z | |
dc.date.issued | 2016-01-30 | |
dc.description.abstract | ZnO nanotube growth onto Florine Tin Oxide (FTO) was successfully carried out by the hydrothermal method. The effect of annealing temperature was evaluated using several methods : Field Emission Scanning Electron Microscopy (FESEM) and Energy Dispersive X-Ray (EDX). The FESEM images showed ZnO nanotubes with a slighty different size of diameter grown on the substrate. The EDX study confirmed the presence of Zn shown by the three peaks of 1 keV, 8.60 keV, and 9.60 keV, while the presence of B was confirmed by the peak of 0.16 keV. The EDX also informed physically quantified percentage of Zn and O are representiedly the weight percentage of 71.22 % and 3.72 % and atomic percentage of 35.40 % and 11.18 %. | en_US |
dc.description.sponsorship | Fakultas Matematika dan Ilmu Pengetahuan Alam Universitas Riau | en_US |
dc.identifier.other | wahyu sari yeni | |
dc.identifier.uri | http://repository.unri.ac.id/xmlui/handle/123456789/7841 | |
dc.language.iso | en | en_US |
dc.subject | DSSC | en_US |
dc.subject | ZnO Nanostructure | en_US |
dc.subject | Hidrothermal | en_US |
dc.subject | Boron | en_US |
dc.title | Efek Variasi Suhu Annealing Terhadap Morfologi Nanotube ZnO yang Di-doping Boron | en_US |
dc.type | student Paper Post Degree | en_US |