Efek Variasi Suhu Annealing Terhadap Morfologi Nanotube ZnO yang Di-doping Boron

No Thumbnail Available

Date

2016-01-30

Journal Title

Journal ISSN

Volume Title

Publisher

Abstract

ZnO nanotube growth onto Florine Tin Oxide (FTO) was successfully carried out by the hydrothermal method. The effect of annealing temperature was evaluated using several methods : Field Emission Scanning Electron Microscopy (FESEM) and Energy Dispersive X-Ray (EDX). The FESEM images showed ZnO nanotubes with a slighty different size of diameter grown on the substrate. The EDX study confirmed the presence of Zn shown by the three peaks of 1 keV, 8.60 keV, and 9.60 keV, while the presence of B was confirmed by the peak of 0.16 keV. The EDX also informed physically quantified percentage of Zn and O are representiedly the weight percentage of 71.22 % and 3.72 % and atomic percentage of 35.40 % and 11.18 %.

Description

Keywords

DSSC, ZnO Nanostructure, Hidrothermal, Boron