SINTESIS KOBAL OKSIDA (Co3O4) DAN UJI DEGRADASI PADA METANIL KUNING
dc.contributor.author | Prasanti, Astarina Atik | |
dc.contributor.author | Mukhtar, Akmal | |
dc.contributor.author | Yanti, Pepi Helza | |
dc.date.accessioned | 2016-05-16T03:40:54Z | |
dc.date.available | 2016-05-16T03:40:54Z | |
dc.date.issued | 2016-05-16 | |
dc.description.abstract | The synthesis of cobalt oxides by precipitation method have been done. (Co(NO3)2.6H2O and KOH was used as precursors in synthesis. Molar ratio of precursors 1:1 M. Temperature of calcination at 900oC was done to deteminate the crystalinity of cobalt oxides. The powder obtained were analyzed using XRD, size of particle of cobalt oxide was examined with Scherrer equation. The result revealed that temperature of calcination at 900 oC have highest intensity of Co3O4 minerals and size of particle was 40,47 nm. The optimum of time irradiation at 60 minute with mass of Co3O4 0,008 g the percentage is 20,06. | en_US |
dc.description.sponsorship | Fakultas Matematika dan Ilmu Pengetahuan Alam Universitas Riau | en_US |
dc.identifier.issn | wahyu sari yeni | |
dc.identifier.uri | http://repository.unri.ac.id/xmlui/handle/123456789/8381 | |
dc.language.iso | en | en_US |
dc.subject | Cobalt oxide | en_US |
dc.subject | precipitation | en_US |
dc.subject | metanil yellow | en_US |
dc.subject | degradation | en_US |
dc.title | SINTESIS KOBAL OKSIDA (Co3O4) DAN UJI DEGRADASI PADA METANIL KUNING | en_US |
dc.type | student Paper Post Degree | en_US |
Files
Original bundle
1 - 1 of 1
No Thumbnail Available
- Name:
- SINTESIS KOBAL OKSIDA DAN UJI PADA DEGRADASI METANIL KUNING.pdf
- Size:
- 683.6 KB
- Format:
- Adobe Portable Document Format
- Description:
- artikel
License bundle
1 - 1 of 1
No Thumbnail Available
- Name:
- license.txt
- Size:
- 1.71 KB
- Format:
- Item-specific license agreed upon to submission
- Description: