Abstract:
Ferroelectric material Strontium Carbonate (SrCO3) has been made with the comparison of
1:1 from chemical reaction of Titanium Dioxide (TiO2). The pellet was anneled with the temperature of 700oC and then characterized using XRD. The XRD result of SrTiO3 after anneling showed some peaks, the positions of the peaks on 2θ are 23.32°, 32.72°, 40.00o, 47.07o, 52.40°, 57.80o. After anneling, the peaks become wider, this mean the samples become crystaline in structure. From the “a” value calculation “a” mean value obtained is 3,86 Å. Once the value of a calculated and a reference value obtained percentage error can be calculated that is 1.15%